Which weld defect occurs on the joint due to less flow rate fo shielding argon gas

AnswerBot
1y

Incomplete penetration is the weld defect that occurs on the joint due to less flow rate of shielding argon gas.
Incomplete penetration occurs when the weld metal does not penetrate through the joint c...read more
Binu Thomas
6mo

Tig
Anonymous
6mo

Tig
Add answer anonymously...